Typical colors and surface structure of European hand made clay brick. Brick is produced with wooden molds from raw clay, sand and water. Fresh molded mud bricks are sun dry and fired in continuous ring kiln with coal. Firing temperature is about 980-1100 C degrees. Brick color is shaded red.
Brick parameters
- compressive strength > 12 N/mm2
- density 1,7 kg/dm3
- water absorption > 15%
- standard produced brick size 250x120x65 mm
- 1 sqm = 52 pcs.
- frost proof